- 件名Nanoindentation Material properties Die cast aluminum alloy Surrogate model Finite-element analysis...
デジタル記事
インターネットで読める全国の図書館
- 要約等In theory, identification of material properties of microscopic materials, such as thin...... by simulation and optimization t...... with a number of finite element......er proposes an identification methodology based on nanoindentation that aims at a......a small number of finite element......e construction of a surrogate model using artificial neu......ve the quality of the surrogate model. In addi......o identify the material parameters that match the surrogate model with the......rated with the nanoindentation of an aluminum ma......nal efficiency and accuracy.
- 標準番号(その他)https://hdl.handle.net/2324/1811127
- 件名Nanoindentation Material properties Die cast aluminum alloy Surrogate model Finite-element analysis...